Abstract

Background

The purpose of this study is to evaluate the wear and fracture strength of crowns and three-unit partial fixed dental prosthesis (FDP) fabricated using by Bruxzir and Incoris TZI as recently introduced monolithic zirconia materials.

Methods

A total of sixteen crowns and sixteen three-unit FDPs were fabricated using Bruxzir and Incoris TZI (n = 8). All specimens were subjected to a 2-body wear test in a dual axis chewing simulator for 1,200,000 loading cycles against steatite antagonist balls. The fracture strength and volumetric loss were recorded. The obtained data were statistically analyzed by 2-way ANOVA testing (α = 0.05).

Results

The mean volumetric loss of the crowns was higher than that of the three-unit FDPs (p < 0.05). Of the two monolithic systems, Incoris TZI exhibited more wear than Bruxzir. The fracture strengths of Bruxzir crowns and FDPs were found to be higher than those of the crowns and FDPs fabricated with Incoris TZI (p < 0.05).

Conclusion

In in vitro test conditions, Bruxzir and Incoris TZI monolithic zirconia systems are fracture-resistant for the crown and FDP application against physiologic chewing forces owing to dynamic aging. Among newly developed monolithic zirconia materials, Bruxzir is found to be more resistant to fracture compared to the Incoris TZI.
Literature
2.
go back to reference Raut A, Rao PL, Ravindranath T. Zirconium for esthetic rehabilitation: an overview. Indian J Dent Res. 2011;22:140–3.CrossRefPubMed Raut A, Rao PL, Ravindranath T. Zirconium for esthetic rehabilitation: an overview. Indian J Dent Res. 2011;22:140–3.CrossRefPubMed
3.
go back to reference Seghi RR, Rosenstial SF, Bauer P. Abrasion of human enamel by different dental ceramics in vitro. J Dent Res. 1991;70:221–5.CrossRefPubMed Seghi RR, Rosenstial SF, Bauer P. Abrasion of human enamel by different dental ceramics in vitro. J Dent Res. 1991;70:221–5.CrossRefPubMed
4.
go back to reference De Boever JA, McCall WDJ, Holden S, Ash MMJ. Functional occlusal forces: an investigation by telemetry. J Prosthet Dent. 1978;40:326–33.CrossRefPubMed De Boever JA, McCall WDJ, Holden S, Ash MMJ. Functional occlusal forces: an investigation by telemetry. J Prosthet Dent. 1978;40:326–33.CrossRefPubMed
5.
go back to reference Schindler HJ, Stengel E, Spiess WE. Feedback control during mastication of solid food textures- a clinical experimental study. J Prosthet Dent. 1998;80:330–6.CrossRefPubMed Schindler HJ, Stengel E, Spiess WE. Feedback control during mastication of solid food textures- a clinical experimental study. J Prosthet Dent. 1998;80:330–6.CrossRefPubMed
6.
go back to reference Nishigawa K, Bando E, Nakano M. Quantitative study of bite force during sleep associated bruxism. J Oral Rehabil. 2001;28:485–91.CrossRefPubMed Nishigawa K, Bando E, Nakano M. Quantitative study of bite force during sleep associated bruxism. J Oral Rehabil. 2001;28:485–91.CrossRefPubMed
7.
go back to reference Kohyama K, Hatakeyama E, Sasaki T, Dan H, Azuma T, Karita K. Effects of sample hardness on human chewing force: a model study using silicone rubber. Arch Oral Biol. 2004;49:805–16.CrossRefPubMed Kohyama K, Hatakeyama E, Sasaki T, Dan H, Azuma T, Karita K. Effects of sample hardness on human chewing force: a model study using silicone rubber. Arch Oral Biol. 2004;49:805–16.CrossRefPubMed
8.
go back to reference Cosme DC, Baldisserotto SM, Canabarro SA, Shinkai RS. Bruxism and voluntary maximal bite force in young dentate adults. Int J Prosthodont. 2005;18:328–32.PubMed Cosme DC, Baldisserotto SM, Canabarro SA, Shinkai RS. Bruxism and voluntary maximal bite force in young dentate adults. Int J Prosthodont. 2005;18:328–32.PubMed
9.
go back to reference DeLong R, Douglas WH. An artificial oral environment for testing dental materials. IEEE Trans Biomed Eng. 1991;38:339–45.CrossRefPubMed DeLong R, Douglas WH. An artificial oral environment for testing dental materials. IEEE Trans Biomed Eng. 1991;38:339–45.CrossRefPubMed
10.
go back to reference Kern M, Strub JR, Lü XY. Wear of composite resin veneering materials in a dual-axis chewing simulator. J Oral Rehabil. 1999;26:372–8.CrossRefPubMed Kern M, Strub JR, Lü XY. Wear of composite resin veneering materials in a dual-axis chewing simulator. J Oral Rehabil. 1999;26:372–8.CrossRefPubMed
11.
go back to reference Delong R, Douglas WH. Development of an artificial oral environment for testing of dental restoratives: biaxial force and movement control. J Dent Res. 1983;62:32–6.CrossRefPubMed Delong R, Douglas WH. Development of an artificial oral environment for testing of dental restoratives: biaxial force and movement control. J Dent Res. 1983;62:32–6.CrossRefPubMed
12.
go back to reference Kheradmandan S, Koutayas SO, Bernhard M, Strub JR. Fracture strength of four different types of anterior 3-unit bridges after thermomechanical fatigue in the dual-axis chewing simulator. J Oral Rehabil. 2001;28:361–9.CrossRefPubMed Kheradmandan S, Koutayas SO, Bernhard M, Strub JR. Fracture strength of four different types of anterior 3-unit bridges after thermomechanical fatigue in the dual-axis chewing simulator. J Oral Rehabil. 2001;28:361–9.CrossRefPubMed
13.
go back to reference Heintze SD, Albrecht T, Cavalleri A, Steiner M. A new method to test the fracture probability of all-ceramic crowns with a dual-axis chewing simulator. Dent Mater. 2011;27:10–9.CrossRef Heintze SD, Albrecht T, Cavalleri A, Steiner M. A new method to test the fracture probability of all-ceramic crowns with a dual-axis chewing simulator. Dent Mater. 2011;27:10–9.CrossRef
14.
go back to reference Preis V, Weiser F, Handel G, Rosentritt M. Wear performance of monolithic dental ceramics with different surface treatments. Quintessence Int. 2013;44:393–405.PubMed Preis V, Weiser F, Handel G, Rosentritt M. Wear performance of monolithic dental ceramics with different surface treatments. Quintessence Int. 2013;44:393–405.PubMed
15.
go back to reference D’Arcangelo C, Vanini L, Rondoni GD, Pirani M, Vadini M, Gattone M, et al. Wear properties of dental ceramics and porcelains compared with human enamel. J Prosthet Dent. 2016;115:350–5.CrossRefPubMed D’Arcangelo C, Vanini L, Rondoni GD, Pirani M, Vadini M, Gattone M, et al. Wear properties of dental ceramics and porcelains compared with human enamel. J Prosthet Dent. 2016;115:350–5.CrossRefPubMed
16.
go back to reference Heintze SD, Eser A, Monreal D, Rousson V. Using a chewing simulator for fatigue testing of metal ceramic crowns. J Mech Behav Biomed Mater. 2017;65:770–80.CrossRefPubMed Heintze SD, Eser A, Monreal D, Rousson V. Using a chewing simulator for fatigue testing of metal ceramic crowns. J Mech Behav Biomed Mater. 2017;65:770–80.CrossRefPubMed
17.
go back to reference Rosentritt M, Behr M, Gebhard R, Handel G. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dent Mater. 2006;22:176–82.CrossRefPubMed Rosentritt M, Behr M, Gebhard R, Handel G. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dent Mater. 2006;22:176–82.CrossRefPubMed
18.
go back to reference Rosentritt M, Behr M, Scharnagl P, Handel G, Kolbeck C. Influence of resilient support of abutment teeth on fracture resistance of all-ceramic fixed partial dentures: an in-vitro study. Int J Prosthodont. 2011;24:465–8.PubMed Rosentritt M, Behr M, Scharnagl P, Handel G, Kolbeck C. Influence of resilient support of abutment teeth on fracture resistance of all-ceramic fixed partial dentures: an in-vitro study. Int J Prosthodont. 2011;24:465–8.PubMed
19.
go back to reference Stappert CF, Att W, Gerds T, Strub JR. Fracture resistance of different partial-coverage ceramic molar restorations: An in vitro investigation. J Am Dent Assoc. 2006;137:514–22.CrossRefPubMed Stappert CF, Att W, Gerds T, Strub JR. Fracture resistance of different partial-coverage ceramic molar restorations: An in vitro investigation. J Am Dent Assoc. 2006;137:514–22.CrossRefPubMed
20.
21.
go back to reference Singhatanagit W, Junkaev P, Singhatanagit P. Effect of bidirectional loading on contact and force characteristics under a newly developed masticatory simulator with a dual-direction loading system. Dent Mater J. 2016;35:952–61.CrossRef Singhatanagit W, Junkaev P, Singhatanagit P. Effect of bidirectional loading on contact and force characteristics under a newly developed masticatory simulator with a dual-direction loading system. Dent Mater J. 2016;35:952–61.CrossRef
22.
go back to reference Rosenstiel SF, Land MF, Crispin BJ. Dental luting agents: a review of current literature. J Prosthet Dent. 1998;80:280–301.CrossRefPubMed Rosenstiel SF, Land MF, Crispin BJ. Dental luting agents: a review of current literature. J Prosthet Dent. 1998;80:280–301.CrossRefPubMed
23.
go back to reference Burke FJ, Fleming GJ, Nathanson D, Marquis PM. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent. 2002;4:7–22.PubMed Burke FJ, Fleming GJ, Nathanson D, Marquis PM. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent. 2002;4:7–22.PubMed
24.
go back to reference Raigrodski A. Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature. J Prosthet Dent. 2001;92:557–62.CrossRef Raigrodski A. Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature. J Prosthet Dent. 2001;92:557–62.CrossRef
25.
go back to reference Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina, feldspar, leucite, mica, and zirconia-based ceramics. J Dent. 2000;28:529–35.CrossRefPubMed Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina, feldspar, leucite, mica, and zirconia-based ceramics. J Dent. 2000;28:529–35.CrossRefPubMed
26.
go back to reference Eroğlu Z, Gurbulak AG. Fatigue behavior of zirconia-ceramic, Galvano-ceramic, and porcelain-fused-to-metal fixed partial dentures. J Prosthodont. 2013;22:516–22.CrossRefPubMed Eroğlu Z, Gurbulak AG. Fatigue behavior of zirconia-ceramic, Galvano-ceramic, and porcelain-fused-to-metal fixed partial dentures. J Prosthodont. 2013;22:516–22.CrossRefPubMed
27.
go back to reference DIN EN ISO 22674 Norm. Metallic materials for fixed and removable restoration application. Berlin: DIN, German Institute for Norming; 2006. DIN EN ISO 22674 Norm. Metallic materials for fixed and removable restoration application. Berlin: DIN, German Institute for Norming; 2006.
28.
go back to reference Kelly JR, Benetti P, Rungruanganunt P, Bona AD. The slippery slope: critical perspectives on in vitro research methodologies. Dent Mater. 2012;28:41–51.CrossRefPubMed Kelly JR, Benetti P, Rungruanganunt P, Bona AD. The slippery slope: critical perspectives on in vitro research methodologies. Dent Mater. 2012;28:41–51.CrossRefPubMed
29.
go back to reference Mundhe K, Jain V, Pruthi G, Shah N. Clinical study to evaluate the wear of natural enamel antagonist to zirconia and metal ceramic crowns. J Prosthet Dent. 2015;114:358–63.CrossRefPubMed Mundhe K, Jain V, Pruthi G, Shah N. Clinical study to evaluate the wear of natural enamel antagonist to zirconia and metal ceramic crowns. J Prosthet Dent. 2015;114:358–63.CrossRefPubMed
30.
go back to reference Bader G, Lavigne G. Sleep bruxism: an overview of an oromandibular sleep movement disorder. Sleep Med Rev. 2000;4:27–43.CrossRefPubMed Bader G, Lavigne G. Sleep bruxism: an overview of an oromandibular sleep movement disorder. Sleep Med Rev. 2000;4:27–43.CrossRefPubMed
31.
go back to reference Chitmongkolsuk S, Heydecke G, Stappert C, Strub JR. Fracture strength of all-ceramic lithium disilicate and porcelain-fused-to-metal bridges for molar replacement after dynamic loading. Eur J Prosthodont Restor Dent. 2002;10:15–22.PubMed Chitmongkolsuk S, Heydecke G, Stappert C, Strub JR. Fracture strength of all-ceramic lithium disilicate and porcelain-fused-to-metal bridges for molar replacement after dynamic loading. Eur J Prosthodont Restor Dent. 2002;10:15–22.PubMed
32.
go back to reference Beuer F, Steff B, Naumann M, Sorensen JA. Load-bearing capacity of all-ceramic three-unit fixed partial dentures with different computer-aided design (CAD)/computer-aided manufacturing (CAM) fabricated framework materials. Eur J Oral Sci. 2008;116:381–6.CrossRefPubMed Beuer F, Steff B, Naumann M, Sorensen JA. Load-bearing capacity of all-ceramic three-unit fixed partial dentures with different computer-aided design (CAD)/computer-aided manufacturing (CAM) fabricated framework materials. Eur J Oral Sci. 2008;116:381–6.CrossRefPubMed
33.
go back to reference Kohorst P, Dittmer MP, Borchers L, Stiesch-Scholz M. Influence of cyclic fatigue in water on the load-bearing capacity of dental bridges made of zirconia. Acta Biomater. 2008;4:1140–7.CrossRef Kohorst P, Dittmer MP, Borchers L, Stiesch-Scholz M. Influence of cyclic fatigue in water on the load-bearing capacity of dental bridges made of zirconia. Acta Biomater. 2008;4:1140–7.CrossRef
34.
go back to reference Schultheis S, Strub JR, Gerds TA, Guess PC. Monolithic and bi-layered CAD/CAM lithium –disilicate versus metal-ceramic fixed dental prostheses: comparison of fracture loads and failure modes after fatigue. Clin Oral Invest. 2013;17:1407–13.CrossRef Schultheis S, Strub JR, Gerds TA, Guess PC. Monolithic and bi-layered CAD/CAM lithium –disilicate versus metal-ceramic fixed dental prostheses: comparison of fracture loads and failure modes after fatigue. Clin Oral Invest. 2013;17:1407–13.CrossRef
35.
go back to reference D’Arcangelo C, Vanini L, Rondoni GD, De Angelis F. Wear properties of a novel resin composite compared to human enamel and other restorative materials. Oper Dent. 2014;39:612–8.CrossRefPubMed D’Arcangelo C, Vanini L, Rondoni GD, De Angelis F. Wear properties of a novel resin composite compared to human enamel and other restorative materials. Oper Dent. 2014;39:612–8.CrossRefPubMed
37.
go back to reference Luthardt RG, Bornemann G, Lemelson S, Walter MH, Hüls A. An innovative method for evaluation of the 3-D internal fit of CAD/CAM crowns fabricated after direct optical versus indirect laser scan digitizing. Int J Prosthodont. 2004;17:680–5.PubMed Luthardt RG, Bornemann G, Lemelson S, Walter MH, Hüls A. An innovative method for evaluation of the 3-D internal fit of CAD/CAM crowns fabricated after direct optical versus indirect laser scan digitizing. Int J Prosthodont. 2004;17:680–5.PubMed
38.
go back to reference Oh W, Anusavice KJ. Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures. J Prosthet Dent. 2002;87:536–42.CrossRefPubMed Oh W, Anusavice KJ. Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures. J Prosthet Dent. 2002;87:536–42.CrossRefPubMed
Metadata
Title
Effects of dynamic aging on the wear and fracture strength of monolithic zirconia restorations
Authors
Işıl Sarıkaya
Yeliz Hayran
Publication date
01-12-2018
Publisher
BioMed Central
Published in
BMC Oral Health / Issue 1/2018
Electronic ISSN: 1472-6831
DOI
https://doi.org/10.1186/s12903-018-0618-z

Other articles of this Issue 1/2018

BMC Oral Health 1/2018 Go to the issue