Abstract

Objectives

This study aims to evaluate the influence of different surface preparation techniques on long-term bonding effectiveness to eroded dentin.

Materials and methods

Dentin specimens were eroded by pH cycling or were left untreated as control, respectively. Five different “preparation” techniques were applied: (1) cleaning with pumice, (2) air abrasion, (3) silicon polisher, (4) proxo-shape, and (5) diamond bur. The three-step etch-and-rinse adhesive OptiBond FL (O-FL; Kerr) and the mild two-step self-etch adhesive Clearfil SE Bond (C-SE; Kuraray) were evaluated. Micro-tensile bond strength was measured after water storage for 24 h and 1 year. Fracture analysis was performed by stereomicroscopy and SEM. Interfaces were characterized by TEM. Differences were statistically analyzed with a linear mixed effects model (α = 0.05).

Results

Erosion reduced bond strength in all groups, but this effect was less prominent when eroded dentin was prepared by diamond bur. Storage lowered bond strength in almost all groups significantly, but this ageing effect was more prominent for the eroded surfaces than for non-eroded controls. Whereas after 1-year control specimens revealed superior bond strength with the three-step etch-and-rinse adhesive (O-FL), the mild two-step self-etch adhesive (C-SE) revealed a better 1-year bond strength to eroded dentin. The interface at eroded dentin appeared very prone to degradation as was shown by the increased amount of adhesive failures and by the silver infiltration detected by TEM.

Conclusions and clinical relevance

Although a minimally invasive approach should clinically always be strived for, superficial preparation (or minimal roughening) with a diamond bur is recommendable for long-term bonding to eroded dentin.
Literature
1.
go back to reference Myklebust S, Espelid I, Svalestad S, Tveit AB (2003) Dental health behavior, gastroesophageal disorders and dietary habits among Norwegian recruits in 1990 and 1999. Acta Odontol Scand 61:100–104PubMedCrossRef Myklebust S, Espelid I, Svalestad S, Tveit AB (2003) Dental health behavior, gastroesophageal disorders and dietary habits among Norwegian recruits in 1990 and 1999. Acta Odontol Scand 61:100–104PubMedCrossRef
2.
go back to reference Karamanolis G, Sifrim D (2007) Developments in pathogenesis and diagnosis of gastroesophageal reflux disease. Curr Opin Gastroenterol 23:428–433PubMedCrossRef Karamanolis G, Sifrim D (2007) Developments in pathogenesis and diagnosis of gastroesophageal reflux disease. Curr Opin Gastroenterol 23:428–433PubMedCrossRef
3.
go back to reference Waterhouse PJ, Auad SM, Nunn JH, Stehen IN, Moynihan PJ (2008) Diet and dental erosion in young people in south-east Brazil. Int J Paediatr Dent 18:353–360PubMedCrossRef Waterhouse PJ, Auad SM, Nunn JH, Stehen IN, Moynihan PJ (2008) Diet and dental erosion in young people in south-east Brazil. Int J Paediatr Dent 18:353–360PubMedCrossRef
4.
go back to reference Brunton PA, Kalsi KS, Watts DC, Wilson NH (2000) Resistance of two dentin-bonding agents and a dentin desensitizer to acid erosion in vitro. Dent Mater 16:351–355PubMedCrossRef Brunton PA, Kalsi KS, Watts DC, Wilson NH (2000) Resistance of two dentin-bonding agents and a dentin desensitizer to acid erosion in vitro. Dent Mater 16:351–355PubMedCrossRef
5.
go back to reference Azzopardi A, Bartlett SW, Watson TF, Sheriff M (2001) The measurement and prevention of erosion and abrasion. J Dent 29:295–400CrossRef Azzopardi A, Bartlett SW, Watson TF, Sheriff M (2001) The measurement and prevention of erosion and abrasion. J Dent 29:295–400CrossRef
6.
go back to reference Sundaram G, Wilson R, Watson TF, Bartlett D (2007) Clinical measurement of palatal tooth wear following coating by a resin sealing system. Oper Dent 32:539–543PubMedCrossRef Sundaram G, Wilson R, Watson TF, Bartlett D (2007) Clinical measurement of palatal tooth wear following coating by a resin sealing system. Oper Dent 32:539–543PubMedCrossRef
7.
go back to reference Azzopardi A, Bartlett DW, Watson TF, Sheriff M (2004) The surface effects of erosion and abrasion on dentine with and without a protective layer. Br Dent J 96:341–354 Azzopardi A, Bartlett DW, Watson TF, Sheriff M (2004) The surface effects of erosion and abrasion on dentine with and without a protective layer. Br Dent J 96:341–354
8.
go back to reference Federlin M, Thonemann B, Schmalz G, Urlinger T (1998) Clinical evaluation of different adhesive systems for restoring teeth with erosion lesions. Clin Oral Investig 2:58–66PubMedCrossRef Federlin M, Thonemann B, Schmalz G, Urlinger T (1998) Clinical evaluation of different adhesive systems for restoring teeth with erosion lesions. Clin Oral Investig 2:58–66PubMedCrossRef
9.
go back to reference Brackett WW, Brackett MG, Dib A, Franco G, Estudillo H (2005) Eighteen-month clinical performance of a self-etching primer in unprepared class V resin restorations. Oper Dent 30:424–429PubMed Brackett WW, Brackett MG, Dib A, Franco G, Estudillo H (2005) Eighteen-month clinical performance of a self-etching primer in unprepared class V resin restorations. Oper Dent 30:424–429PubMed
10.
go back to reference Rocha PI, Borges AB, Rodrigues JR, Arrais CA, Giannini M (2006) Effect of dentinal surface preparation on bond strength of self etching adhesive systems. Braz Oral Res 20:52–58PubMedCrossRef Rocha PI, Borges AB, Rodrigues JR, Arrais CA, Giannini M (2006) Effect of dentinal surface preparation on bond strength of self etching adhesive systems. Braz Oral Res 20:52–58PubMedCrossRef
11.
go back to reference Sattabanasuk V, Vachiramon V, Qian F, Armstrong SR (2007) Resin–dentin bond strength as related to different surface preparation methods. J Dent 35:467–475PubMedCrossRef Sattabanasuk V, Vachiramon V, Qian F, Armstrong SR (2007) Resin–dentin bond strength as related to different surface preparation methods. J Dent 35:467–475PubMedCrossRef
12.
go back to reference Ermis RB, De Munck J, Cardoso MV, Coutinho E, van Landuyt KL, Poitevin A, Lambrechts P, Van Meerbeek B (2008) Bond strength of self-etch adhesives to dentin prepared with three different diamond burs. Dent Mater 24:978–985PubMedCrossRef Ermis RB, De Munck J, Cardoso MV, Coutinho E, van Landuyt KL, Poitevin A, Lambrechts P, Van Meerbeek B (2008) Bond strength of self-etch adhesives to dentin prepared with three different diamond burs. Dent Mater 24:978–985PubMedCrossRef
13.
go back to reference Cardoso MV, Coutinho E, Ermis RB, Poitevin A, Van Landuyt K, De Munck J, Carvalho RCR, Van Meerbeek B (2008) Influence of dentin cavity surface finishing on micro-tensile bond strength of adhesives. Dent Mater 24:492–501PubMedCrossRef Cardoso MV, Coutinho E, Ermis RB, Poitevin A, Van Landuyt K, De Munck J, Carvalho RCR, Van Meerbeek B (2008) Influence of dentin cavity surface finishing on micro-tensile bond strength of adhesives. Dent Mater 24:492–501PubMedCrossRef
14.
go back to reference Yiu CKY, Hirashi N, King NM, Tay FR (2008) Effect of dentinal surface preparation on bond strength of self-etching adhesives. J Adhes Dent 10:173–182PubMed Yiu CKY, Hirashi N, King NM, Tay FR (2008) Effect of dentinal surface preparation on bond strength of self-etching adhesives. J Adhes Dent 10:173–182PubMed
15.
go back to reference Poitevin A, De Munck J, Van Landuyt K, Coutinho E, Peumans M, Lambrechts P, Van Meerbeek B (2007) Influence of three specimen fixation modes on the micro tensile bond strength of adhesives to dentin. Dent Mater J 26:694–699PubMedCrossRef Poitevin A, De Munck J, Van Landuyt K, Coutinho E, Peumans M, Lambrechts P, Van Meerbeek B (2007) Influence of three specimen fixation modes on the micro tensile bond strength of adhesives to dentin. Dent Mater J 26:694–699PubMedCrossRef
16.
go back to reference Tay FR, Pashley DH, Yoshiyama M (2002) Two modes of nanoleakage expression in single-step adhesives. J Dent Res 81:472–476PubMedCrossRef Tay FR, Pashley DH, Yoshiyama M (2002) Two modes of nanoleakage expression in single-step adhesives. J Dent Res 81:472–476PubMedCrossRef
17.
go back to reference Ganss C, Schlueter N, Hardt M, von Hinckeldey J, Klimek J (2007) Effects of toothbrushing on eroded dentine. Eur J Oral Sci 115:390–396PubMedCrossRef Ganss C, Schlueter N, Hardt M, von Hinckeldey J, Klimek J (2007) Effects of toothbrushing on eroded dentine. Eur J Oral Sci 115:390–396PubMedCrossRef
18.
go back to reference Francisconi LF, Honório HM, Rios D, Maghalães AC, Machado MAAM, Buzalaf MAR (2008) Effect of pH cycling on different restorative materials and on enamel restored with these materials. Oper Dent 33:203–208PubMedCrossRef Francisconi LF, Honório HM, Rios D, Maghalães AC, Machado MAAM, Buzalaf MAR (2008) Effect of pH cycling on different restorative materials and on enamel restored with these materials. Oper Dent 33:203–208PubMedCrossRef
19.
go back to reference Maghalães AC, Rios D, Moino AL, Wiegand A, Attin T, Buzalaf MAR (2008) Effect of different concentrations of fluoride in dentifrices on dentin erosion subjected or not to abrasion in situ/ ex vivo. Caries Res 42:112–116CrossRef Maghalães AC, Rios D, Moino AL, Wiegand A, Attin T, Buzalaf MAR (2008) Effect of different concentrations of fluoride in dentifrices on dentin erosion subjected or not to abrasion in situ/ ex vivo. Caries Res 42:112–116CrossRef
20.
go back to reference Van Meerbeek B, Peumans M, Poitevin A, Mine A, Van Ende A, Neves A, De Munck J (2010) Relationship between bond-strength tests and clinical outcomes. Dent Mater 26:e100–e121PubMedCrossRef Van Meerbeek B, Peumans M, Poitevin A, Mine A, Van Ende A, Neves A, De Munck J (2010) Relationship between bond-strength tests and clinical outcomes. Dent Mater 26:e100–e121PubMedCrossRef
21.
go back to reference Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H (2000) In vivo degradation of resin–dentin bonds in humans over 1 to 3 years. J Dent Res 79:1385–1391PubMedCrossRef Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H (2000) In vivo degradation of resin–dentin bonds in humans over 1 to 3 years. J Dent Res 79:1385–1391PubMedCrossRef
22.
go back to reference De Munck J, Van Landuyt K, Peumans M, Poitevin A, Lambrechts P, Braem M, Van Meerbeek B (2005) A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res 84:118–132PubMedCrossRef De Munck J, Van Landuyt K, Peumans M, Poitevin A, Lambrechts P, Braem M, Van Meerbeek B (2005) A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res 84:118–132PubMedCrossRef
23.
go back to reference Sano H, Takastu T, Ciucchi B, Horner JA, Matthews WG, Pashley DH (1995) Nanoleakage: leakage within the hybrid layer. Oper Dent 20:18–25PubMed Sano H, Takastu T, Ciucchi B, Horner JA, Matthews WG, Pashley DH (1995) Nanoleakage: leakage within the hybrid layer. Oper Dent 20:18–25PubMed
24.
go back to reference Hashimoto M, Ohno H, Sano H, Kaga M, Oguchi H (2003) Degradation patterns of different adhesives and bonding procedures. J Biomed Mater Res 66B:324–330CrossRef Hashimoto M, Ohno H, Sano H, Kaga M, Oguchi H (2003) Degradation patterns of different adhesives and bonding procedures. J Biomed Mater Res 66B:324–330CrossRef
25.
go back to reference Hara AT, Queiroz CS, Giannini M, Cury JA, Serra MC (2004) Influence of the mineral content and morphological pattern of artificial root caries lesion on composite resin bond strength. Eur J Oral Sci 112:67–72PubMedCrossRef Hara AT, Queiroz CS, Giannini M, Cury JA, Serra MC (2004) Influence of the mineral content and morphological pattern of artificial root caries lesion on composite resin bond strength. Eur J Oral Sci 112:67–72PubMedCrossRef
26.
go back to reference Schmidlin PR, Siebenmann J, Kocher P, Seemann R, Attin T, Bindl A (2008) Effects of de- and remineralization of dentin on bond strengths yielded by one-, three, and four step adhesives. J Adhes Dent 10:119–126PubMed Schmidlin PR, Siebenmann J, Kocher P, Seemann R, Attin T, Bindl A (2008) Effects of de- and remineralization of dentin on bond strengths yielded by one-, three, and four step adhesives. J Adhes Dent 10:119–126PubMed
27.
go back to reference De Oliveira MT, de Freitas PM, de Paula EC, Ambrosano GM, Giannini M (2007) Influence of diamond sono-abrasion, air-abrasion and Er:YAG laser irradiation on bonding of different adhesive systems to dentin. Eur J Dent 1:158–166PubMed De Oliveira MT, de Freitas PM, de Paula EC, Ambrosano GM, Giannini M (2007) Influence of diamond sono-abrasion, air-abrasion and Er:YAG laser irradiation on bonding of different adhesive systems to dentin. Eur J Dent 1:158–166PubMed
28.
go back to reference Mine A, De Munck J, Cardoso MV, Van Landuyt KL, Poitevin A, Kuboki T, Yoshida Y, Suzuki K, Van Meerbeek B (2010) Enamel-smear compromises bonding by mild self-etch adhesives. J Dent Res 89:1505–1509PubMedCrossRef Mine A, De Munck J, Cardoso MV, Van Landuyt KL, Poitevin A, Kuboki T, Yoshida Y, Suzuki K, Van Meerbeek B (2010) Enamel-smear compromises bonding by mild self-etch adhesives. J Dent Res 89:1505–1509PubMedCrossRef
29.
go back to reference Oliveira SS, Pugach MK, Hilton JF, Watanabe LG, Marshall SJ, Marshall GW Jr (2003) The influence of the dentin smear layer on adhesion: a self-etching primer vs. a total etch system. Dent Mater 19:758–767PubMedCrossRef Oliveira SS, Pugach MK, Hilton JF, Watanabe LG, Marshall SJ, Marshall GW Jr (2003) The influence of the dentin smear layer on adhesion: a self-etching primer vs. a total etch system. Dent Mater 19:758–767PubMedCrossRef
30.
go back to reference De Munck J, Van Meerbeek B, Yoshida Y, Inoue S, Vargas M, Suzuki K, Lambrechts P, Vanherle G (2003) Four-year water degradation of total-etch adhesives bonded to dentin. J Dent Res 82:136–140PubMedCrossRef De Munck J, Van Meerbeek B, Yoshida Y, Inoue S, Vargas M, Suzuki K, Lambrechts P, Vanherle G (2003) Four-year water degradation of total-etch adhesives bonded to dentin. J Dent Res 82:136–140PubMedCrossRef
Metadata
Title
Long-term bonding to eroded dentin requires superficial bur preparation
Authors
Brigitte Zimmerli
Jan De Munck
Adrian Lussi
Paul Lambrechts
Bart Van Meerbeek
Publication date
01-10-2012
Publisher
Springer-Verlag
Published in
Clinical Oral Investigations / Issue 5/2012
Print ISSN: 1432-6981
Electronic ISSN: 1436-3771
DOI
https://doi.org/10.1007/s00784-011-0650-8

Other articles of this Issue 5/2012

Clinical Oral Investigations 5/2012 Go to the issue